Brick/Mortar Compatibility Research Continues

Words: Bijan AalamiMany model building codes require that brick with an initial rate of absorption (IRA) greater than 30 gm/min/30 sq. in. be wetted before laying. This is to prevent the mortar from drying too rapidly. The loss of water from the mortar may result in incomplete hydration of the cement. This is thought to result in lower flexural bond strength and walls with greater water penetration.

The building codes do not differentiate between mortar cementitious materials nor mortar type. Proper wetting of the brick is difficult to achieve and is often ignored by the mason. There is no accepted method of wetting the brick.

The Brick Institute of America (BIA), the Portland Cement Association (PCA), and the National Lime Association (NLA) have joined to evaluate the performance of high IRA brick with a variety of mortar cementitious materials and mortar types. This investigation is similar to a study completed in 1995 on brick with an IRA of 5 or less. The objective of both programs is to identify those mortar materials and types which are most compatible with brick of a given IRA.

Brick selected for this study will be all 100% solid units with wire cut bed surfaces. Mortars will be mixed by proportions using cementitious materials predominant in the Chicago area. Mortar water content will be set by the mason. Tests will be run to determine typical physical properties of all materials.

Flexural unit strength will be evaluated using ASTM C1072. The combinations of materials shown in Table I will be tested. The 45 - 50 gm brick will be laid in both dry and wetted conditions.

The results of the flexural bond tests will be used to select unit/mortar combinations for ASTM E514 water penetration tests. The combination of brick and mortar types that give the highest and lowest bond strength values will be tested.

The brick with the 15 - 20 gm IRA will serve as a basis of comparison. It is the same brick used in the low IRA brick tests run earlier. Thus, this series of tests complements the earlier research.

Table I. Bond Wrench Matrix

Unit IRA gm per min per 30 sq. in. Cementitious Material and Mortar Type
Portland Cement/Lime Mortar Cement Masonry Cement
S N O S N S N
15 - 20   X   X X X X
25 - 30 X X X   X X X
45 - 50 X X X X X X X
From Day One to Long-Term Success: Onboarding Strategies for Contractors
January 2026

The construction industry is facing one of its toughest challenges in decades. Companies are struggling to find enough skilled workers while competing to keep the ones they have. At the same time, projects are becoming more complex, deadlines are tighter,

Finding the Right PPE for Your Work
January 2026

When it comes to PPE, one thing’s for sure: safety isn’t one size fits all. The work you’re doing, where you’re doing it, and even what time of year it is, can all make a big difference in what gear actually works. Price, comfort, and job performance all

Back Injuries: The Real Cost and How to Prevent Them
January 2026

The mention of back injuries makes mason contractors cringe, and for good reason. Masons lift heavy objects every day, all day long. When a person sustains a back injury, it is serious. It affects every part of their life, from their ability to perform wo

Detailing for Durability: The 2026 Guide to High-Performance Stone Veneer Transitions
January 2026

Some of the most expensive failures involving manufactured stone veneer installations don’t come from the stone at all, but rather from the material transitions and flashing around it. Transitions are weak points in the overall cladding where water can fi